Hangzhou Gaoxin Rubber & Plastic Material Co., Ltd.
Products
Contact Us
  • Contact Person : Ms. Zhu erin
  • Company Name : Hangzhou Gaoxin Rubber & Plastic Material Co., Ltd.
  • Tel : 86-571-88581580
  • Fax : 86-571-88501258
  • Address : Zhejiang,Hangzhou,No 10 Longhuang Road,Jingshan Town,Yuhang District,Hangzhou
  • Country/Region : China
  • Zip : 311116

EPDM insulating rubber compound

EPDM insulating rubber compound
Product Detailed
Related Categories:EPDM
1.RoHS environmental protection requirements 2.Excellent product quality

EPDM insulating rubber compound is based on EPDM rubber,is mixed by various additives,such as softener,accelerator,active agents,antioxidants,reinforcing agents,curing agents and so on.Obtaining the compound by mixing,filtering and tableting.

1.APPLICATION

NO.TYPEPRODUCT NAMEAllowable operating temperature of the conductive coreAPPLICATION
1XJ-10A

70°C EPDM insulating rubber compound

70°C

Used for insulating rubber compound at the maximum operating temperature of 70°C

2XJ-30A

90°C  EPDM insulating rubber compound

 
90°C  

Used for mining cables, wind power cables, marine cables at the maximum operating temperature of 90°C

3XJ-80A

Silicon rubber insulating compound or jacket compound

 
180°C  

Used for silicon rubber cables at the maximum operating temperature of 180°C

4XJ-VDE

VDE special rubber insulating compound

 
70°C  

Used for VDE rubber cables 

5XJ-125

Halogen-free flame-retardant rubber insulating compound for vehicles

 
125°C  

Used for vehicles cable

6IE4

General rubber cable insulating compound

 
70°C  

Used for move rubber flexible cable insulating compound 

7XJ-30A(HIGH VOLTAGE) 

10KV rubber cable insulating compound

 
70°C  

Used for 10kV rubber cable

2.INDICATOR

NO.ITEMUNITXJ-10AXJ-30AXJ-80AXJ-VDEXJ-125IE4XJ-30A(HIGH VOLTAGE) 
1Volume resistance rate at 20°C MINΩ.m1x10131x10131x10131x10121x10131x10125x1013
2Dielectric strength MIN MV/m25252520252025
Mechanical properties before aging Tensile strength MINMPa676.561067
Tensile strain at break MIN%250250200250150250250
4     Properties after aging in air oven     Temperature°C100135200100158100135
Timeh168168240168168168168
Tensile strength MINMPa5644.2——4.26
Rate of change%±25±30——±25±10±25±30
Elongation at break MIN%220——120200——200——
Rate of change%±25 ±30——±25±30±25±30
5     Properties after aging in air circumstance    Temperature°C 127127127127127127127
Time40404040404040
Tensile strength MINMPa ——————————————
Rate of change %±30 ±30±30±30±30±30±30
Elongation at break MIN %——————————————
Rate of change %±30 ±30±30±30±30±30±30
6Hot set elongationTemperature°C 200250200200200200250
Load timeMin15151515151515
Mechanical stressN/cm220202020202020
Elongation under load MAX%100175100100100100175
Permanent deformation MAX%2525252525 2525
Ozone resistance Ozone concentration%0.0250.0250.0250.0250.0250.0250.025
Timeh30303030303030
Surface change——No crakeNo crakeNo crakeNo crakeNo crakeNo crakeNo crake
8Mooney viscosity MAX (1+4/100)ML6060 60 60 60 60 60 

NOTE:1.The above models are in line with RoHS environmental protection requirenment,the XJ-VDE comply with REACH and RoHS requirements.

           2.The sulfide way of the above models is steam continuous vulcanization,also we can provide radiation cross-linking to customer requirements.